Products
Dowanol DPM Glycol Ether
- Product Name: Dowanol DPM Glycol Ether
- Factroy Site: No. 100, Qinhuai Road, Jiangning District, Nanjing, Jiangsu, China
- Price Inquiry: sales5@ascent-chem.com
- Manufacturer: Dow Chemical
- CONTACT NOW
- In terms of specification, Dowanol DPM Glycol Ether is supplied with ≥99.0% purity and ≤0.10% water content, making it suitable for water-based coating and industrial cleaning formulations.
| HS Code | 876900 |
| Chemicalname | Dipropylene glycol methyl ether |
| Casnumber | 34590-94-8 |
| Ecnumber | 252-104-2 |
| Molecularformula | C7H16O3 |
| Molecularweight | 148.20 g/mol |
| Appearance | Clear, colorless liquid |
| Odor | Mild, ether-like |
| Boilingpoint | Approximately 188-190 °C at 760 mmHg |
| Flashpoint | Approximately 75 °C (closed cup) |
| Density | 0.951 g/cm³ at 20 °C |
| Viscosity | 3.7 mPa·s at 25 °C |
| Watersolubility | Miscible |
| Vaporpressure | Approximately 0.3 mmHg at 20 °C |
| Autoignitiontemperature | Approximately 205 °C |
As an accredited Dowanol DPM Glycol Ether factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dowanol DPM Glycol Ether packaged in 200-liter steel drums, each drum containing 200 liters for industrial handling. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): 20′ FCL container loaded with Dowanol DPM Glycol Ether, properly stowed, secured, and sealed for ocean shipment. |
| Shipping | Dowanol DPM Glycol Ether is generally shipped as a non-regulated combustible liquid in DOT/UN-approved drums, IBCs, or tank trucks. Keep containers closed, label per SDS, avoid ignition sources, and store in cool, dry, ventilated areas. Shipping papers should include product name, quantity, and applicable safety/regulatory information. |
| Storage | Store Dowanol DPM Glycol Ether in a cool, dry, well-ventilated, fire-resistant area away from heat, sparks, flames, and strong oxidizers. Keep containers tightly closed, labeled, and upright on compatible shelving with secondary containment. Protect from sunlight. Use approved containers and compatible materials; segregate from acids and bases. Provide grounding/bonding for transfers, maintain spill kits and ventilation, and inspect regularly for leaks. |
| Shelf Life | Dowanol DPM Glycol Ether typically has a shelf life of 24 months from manufacture when stored in original, unopened containers under normal conditions. |
Formulation of low-odour interior latex paints below 50 g/L VOC requires a coalescent that partitions sufficiently into the polymer phase to depress minimum film-forming temperature without becoming a permanent plasticizer. Dowanol DPM, a dipropylene glycol methyl ether mixture with a boiling point of 190 °C, density of 0.951 g/cm³ at 20 °C, kinematic viscosity of approximately 4.0 mm²/s at 25 °C, and evaporation rate of 0.035 relative to n-butyl acetate, is used in acrylic, styrene-acrylic, and vinyl acetate-ethylene architectural binders at 2–5 wt% of polymer solids. For semi-gloss and eggshell systems with pigment volume concentration between 25% and 35%, the addition is typically 1–2.5 wt% of total formula. The coalescent is classified as a VOC under US EPA Method 24 because its boiling point is below 250 °C, but its low evaporation rate permits formulation of paints with total VOC below 50 g/L when combined with high-solids dispersions and reactive coalescents. Minimum film-forming temperature depression is measured on the specific latex by ISO 2115; the actual depression is nonlinear and binder-specific, and published data for a given dispersion should be obtained from the polymer supplier rather than estimated from solvent solubility parameters alone. Film properties after 7 days at 23 ± 2 °C and 50 ± 5% relative humidity are evaluated by scrub resistance per ASTM D2486, wet adhesion per ASTM D3359 method B, and washability per ISO 11998. In production, DPM is added during letdown after the millbase has been thinned and pH-adjusted with ammonia or AMP, and before associative thickener addition. A 1,000-L letdown vessel with a 600-mm sawtooth impeller running at 400–600 rpm is adequate; adding DPM directly into a high-shear pigment dispersion can cause binder micro-flocculation, observed as a Hegman gauge drop from 7 NS to 5 NS and a visible loss of tint strength in black masstone rub-outs. Dosage above 7 wt% on binder solids increases early water sensitivity and blocking, measured as a reduction in pendulum hardness under ISO 1522 after 24 h.
| Property | Value | Test method |
|---|---|---|
| Density at 20 °C | 0.951 g/cm³ | ASTM D4052 |
| Kinematic viscosity at 25 °C | 4.0 mm²/s | ASTM D445 |
| Surface tension at 25 °C | 28.8 mN/m | ASTM D1331 |
| Boiling point | 190 °C | ASTM D1078 |
| Flash point, Tag closed cup | 75 °C | ASTM D56 |
| Evaporation rate, n-butyl acetate = 1 | 0.035 | ASTM D3539 |
| Water solubility at 20 °C | complete | visual |
The finished product is an interior premium semi-gloss or eggshell paint for plasterboard, primed wood, and renovated masonry, formulated to meet EU Directive 2004/42/EC phase limits for water-based interior coatings when the DPM content is balanced against other volatile components.
Aqueous 2K Epoxy Shop Primers: Solvent Balance and Induction-Time Control
In waterborne two-component epoxy shop primers applied to blast-prepared steel, Dowanol DPM is used at 2–6 wt% of the mixed primer to bridge the viscosity gap between the epoxy dispersion and the polyamine adduct hardener. The ether alcohol is nonreactive with epoxy-amine chemistry, but its terminal hydroxyl group means that direct substitution into a waterborne 2K polyurethane is not acceptable without compensating the OH/NCO ratio; otherwise hard films develop persistent tack and low pendulum hardness. The standard addition point is the Part A letdown after the grind has been cooled to 40 °C; the batch is then mixed at 500–700 rpm until the Hegman grind remains at 6 NS and the cone/plate viscosity at 10,000 s⁻¹ per ISO 2884-2 falls to 1.0–1.5 Pa·s. On an airless spray line using a 45:1 piston pump and 0.013 in reversible tungsten carbide tip, the reduction in high-shear viscosity lowers spray pressure from approximately 180 bar to 140–150 bar. Field batches exceeding 6 wt% DPM show two defects on vertical steel: sagging during the open time after 600 µm wet film application and a measurable lengthening of through-cure; Konig hardness per ISO 1522 at 24 h can drop from 45 s to 28–32 s. Salt spray testing per ISO 9227 on grit-blasted steel at 100 µm dry film thickness generally remains above 500 h when the primer is applied over Sa 2½ substrate, but the same system at 8 wt% DPM often develops blistering near the scribe within 240 h. The terminal product is a zinc-free shop primer for steel fabrication and structural frames, adjusted with iron oxide and zinc phosphate for flash-rust resistance and applied in a single coat before overcoating with an approved intermediate or topcoat.
Narrow-web flexographic presses running water-based acrylic inks at 120–180 m/min require a slow glycol ether to maintain cell transfer from ceramic anilox rolls without causing blocking on corona-treated polypropylene and high-gloss coated paper. A typical letdown vehicle contains 30–45 wt% styrene-acrylic solution or dispersion, 3–7 wt% Dowanol DPM, 0.5–1.5 wt% ammonia 28%, 2–5 wt% propylene glycol, 0.2–0.5 wt% defoamer, and deionized water to 100 wt%. The DPM is added after the pH is initially raised to 8.5–9.0, but before the final pH correction to 8.8–9.2; addition at high shear with a sawtooth impeller at 1,200 rpm for 10–15 min reduces gel speck formation from pH shock. Final viscosity is adjusted through a 4 mm ISO flow cup at 23 °C to 25–35 s in accordance with ISO 2431. The key production criterion is resolubility: on press stops exceeding 30 min, dried ink on plate and anilox must be removable with a 90/10 water/DPM wash at 500 rpm plate wash cycles, otherwise specking appears in the next print run. Blocking tests on printed film at 40 °C and 0.49 N/cm² for 24 h are used to set the upper DPM limit; concentrations above 7 wt% can soften the dried ink surface and cause adhesion to the reverse side. The finished product is a water-based flexo ink or overprint varnish for non-direct-food-contact folding cartons, snack-food outer wrappers, and paper shopping bags where indirect food contact compliance is evaluated under EU 10/2011 only after migration testing on the final printed structure.
How Does DPM Maintain Phase Stability in Alkaline Hard-Surface Degreasers?
Concentrated alkaline degreasers based on sodium metasilicate and citrate builders are prone to phase separation when nonionic surfactants are salted out; Dowanol DPM acts as a hydrotrope-like coupling solvent that raises the cloud point of the nonionic above the concentrate storage temperature. A representative formula contains 4–8 wt% DPM, 2–5 wt% sodium metasilicate pentahydrate, 3–6 wt% trisodium citrate dihydrate, 2–4 wt% C9–C11 alcohol ethoxylate 6EO, 0.5–1.0 wt% tetrasodium EDTA, and water to 100 wt%. The mixing sequence is stability-critical: DPM is blended with the nonionic surfactant and 10 wt% water at 25–30 °C before the alkaline builder is charged; reverse addition of DPM into a cold gel phase can create a persistent liquid-crystalline lump that requires 2–3 h of low-shear mixing to break. Mixing is carried out in a 2,000-L stainless vessel with a low-rpm turbine at 300–400 rpm; the resulting concentrate has pH 11.2–11.8 and remains clear and pourable down to 5 °C. At use dilution of 1:20 to 1:50, the product removes polymerized grease and carbonized food soil from stainless steel, ceramic, and quarry tile; cleaning performance is evaluated with a Gardco D10 straight-line scrub tester at 30 double rubs and visual rating, with a target of ≥4 on a 1–5 scale. The upper operational boundary is an oxidizer wall: blends with sodium hypochlorite above 5% active chlorine can exotherm and generate degradation byproducts; any use in food-processing areas must be followed by potable-water rinsing and is not a substitute for a separate sanitizing step under DIN EN 1276 or ASTM E1153. The terminal product is an institutional and industrial hard-surface degreaser supplied as a clear concentrate for automatic dilution systems.
Semi-aqueous removal of rosin-based no-clean flux residues from fine-pitch PCB assemblies has shifted from terpene/water emulsions to glycol-ether/water blends because Dowanol DPM provides a surface tension of 28.8 mN/m at 25 °C, solvates abietic acid derivatives without swelling most solder mask polymers, and allows closed-loop recovery at a boiling point of 190 °C. The working bath is composed of 10–20 wt% DPM, 2–5 wt% alkanolamine, 1–3 wt% triazole-based copper corrosion inhibitor, and deionized water; the bath is held at 50–55 °C in a batch cleaner with 40 kHz ultrasonic transducers and power density of 0.8–1.2 W/cm². Cleaning time is 3–5 min, followed by a 2 min rinse in 18 MΩ·cm deionized water at 45 °C and forced-air drying at 70 °C. Ionic cleanliness after cleaning is measured by resistivity of solvent extract under IPC-TM-650 2.3.25; assemblies qualified to IPC J-STD-001 Class 3 generally require values below 1.56 µg NaCl/cm². Production-scale failure modes include excessive attack on bare aluminum wire bond pads when the bath pH exceeds 10 and immersion time extends beyond 5 min; under those conditions, visible etch of Al bond pads occurs with a corresponding drop in wire pull strength per ASTM F459-13. Bath maintenance is by daily gas chromatographic or refractive-index control of DPM concentration, because drag-out losses shift the solvency faster than pH drift. The process is not compatible with polysilicon resonators or exposed copper microvia structures without corrosion inhibitor validation. The terminal product is a cleaned, dry PCB assembly ready for conformal coating, with no chlorinated solvent residue.
High-Electrolyte Emulsifiable Concentrates for Triazole Fungicides
Emulsifiable concentrates of triazole fungicides such as tebuconazole and propiconazole often require a water-miscible co-solvent to prevent crystal growth on dilution into hard water. Dowanol DPM is incorporated at 5–15 wt% of the total formulation, depending on the active loading and the aromatic solvent used; a typical composition is 10–25 wt% active, 2–5 wt% calcium dodecylbenzene sulfonate, 2–5 wt% alcohol ethoxylate, 5–15 wt% DPM, and Solvesso 150 ND to 100 wt%. The manufacturing sequence is the primary control against gel formation: DPM is pre-blended with the oil-soluble surfactants at 30–35 °C, then the molten active at 60–70 °C is added, and the remaining aromatic solvent is metered in after a clear phase forms. High-shear mixing at 3,000–5,000 rpm for 20–30 min in a jacketed vessel with a rotor-stator homogenizer is followed by cooling to 25 °C and filtration through 10 µm polypropylene cartridge filters. The finished product must remain clear after 14 days at 0 °C and must show ≤2% cream separation after 0.5 h in 342 ppm hard water by CIPAC MT36; low-temperature stability is checked by CIPAC MT39.3. In production batches, the most common failure is a pseudoplastic gel that appears when DPM is added directly to the calcium sulfonate before oil dilution; the gel can be reversed by heating to 40 °C and adding the aromatic solvent slowly under low-shear. DPM also raises the flash point of the EC formulation only marginally because the aromatic solvent dominates; the formulated product must still be handled as a flammable liquid under UN 3082 or UN 1993 as classified by the full mixture. The terminal product is an emulsifiable concentrate for foliar and seed-treatment use, with the active solubilized during the initial water dilution at 5 L/ha field rates.
Competitive Dowanol DPM Glycol Ether prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618115175568 or mail to sales5@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618115175568
Email: sales5@ascent-chem.com
Get Free Quote of Dow Chemical
Flexible payment, competitive price, premium service - Inquire now!
- Dowanol DPM Glycol Ether is manufactured under an ISO 9001 quality system and complies with relevant regulatory requirements.
- COA, SDS/MSDS, and related certificates are available upon request. For certificate requests or inquiries, contact: sales5@ascent-chem.com.
What Limits Batch Acceptance in Coating Solvent Receiving?
Incoming inspection protocols at solvent-borne and waterborne coating plants typically apply moisture, acidity, and distillation-range limits before DOWANOL™ DPM is unloaded into stainless steel or lined carbon steel tanks. Water content above 0.10 wt% by ASTM E203 can destabilize moisture-sensitive urethane systems and increase the risk of phase haze in ester-rich industrial coatings. Acidity above 0.01 wt% as acetic acid by ASTM D1613 indicates oxidative degradation or contamination during transit and may accelerate corrosion of unlined steel dosing lines. Color measured by ASTM D1209 is maintained at ≤10 Pt-Co to avoid tint alteration in clear acrylic finishes. Distillation range limits under ASTM D1078, with initial boiling point ≥182 °C and dry point ≤192 °C, provide compositional consistency for evaporation-rate control on high-speed coil coating lines.
| Parameter | Test Method | Specification |
|---|---|---|
| Appearance | Visual inspection | Clear, free of suspended matter |
| Color | ASTM D1209 | ≤10 Pt-Co |
| Purity, normalized GC area | GC-FID internal method | ≥99.0% |
| Water content | ASTM E203 | ≤0.10 wt% |
| Acidity as acetic acid | ASTM D1613 | ≤0.01 wt% |
| Specific gravity at 20/20 °C | ASTM D4052 | 0.947–0.953 |
| Distillation range | ASTM D1078 | IBP ≥182 °C, DP ≤192 °C |
In waterborne architectural and industrial acrylic systems, the coalescing action of DOWANOL™ DPM is governed by plasticization of latex polymer particles and depression of minimum film formation temperature. During production-scale letdown operations using high-torque Cowles dispersers or rotor-stator mixers, the solvent is typically introduced after pigment dispersion and associative thickener hydration to avoid viscosity suppression in the grind phase. Addition before dispersion can reduce shear viscosity and lower energy transfer to pigment agglomerates, prolonging grind time and increasing tint variance between batches. Addition levels of 3–8 wt% on resin solids are conventional for hard acrylic copolymers, but the required dose is resin-specific and is verified by ISO 2115 minimum film formation temperature measurement. Low-shear viscosity is monitored by ASTM D562 Stormer methods, and high-shear viscosity by ASTM D4287 cone-and-plate methods. Dry film hardness and block resistance are evaluated after 7-day conditioning at 23 °C and 50% RH; wet scrub resistance is tested under ASTM D2486. The 0.4 mm Hg vapor pressure at 20 °C yields slower release from the drying film than propylene glycol monomethyl ether, which extends wet-edge time but increases residual solvent at early recoat intervals. In multi-zone drying ovens on flat-line coaters with air temperatures of 50–90 °C, the solvent can be retained in the film if zone exhaust humidity exceeds 60% RH, and tack-free time may exceed equipment dwell. Published data for specific acrylic latex grades remains resin-limited.
Resin Solvency and Evaporation-Rate Gradients in Epoxy and Polyurethane Formulations
Tail-solvent function in high-solids epoxy coatings arises from the balance between the relative evaporation rate of 0.02 (n-butyl acetate = 1) and the polar character required to maintain bisphenol A diglycidyl ether solutions below gel-point viscosity. In two-component polyurethane systems, the molecule’s single secondary hydroxyl group introduces a hydroxyl equivalent weight of approximately 148.2 g/eq and must be counted in NCO:OH stoichiometry when the solvent remains in the film during curing. At 10–15 wt% of total solvent blend, DOWANOL™ DPM may moderate evaporation from static mixer outlet lines, thereby extending pot life and reducing surface skinning, but low-NCO prepolymers can show viscosity drift above 120 min at 25 °C as measurable by ASTM D2196 rotational viscometry. For epoxy vehicles, the solvent is blended with faster ketones or aromatic hydrocarbons to adjust electrical resistivity and surface tension in electrostatic spray operations. Formulators using rotary atomizers with 30–70 kV charging units should verify conductivity by ASTM D4308 because phase separation in high-solids epoxy can shift transfer efficiency. Because the product is hygroscopic, moisture uptake in open process vessels can exceed 0.10 wt% in prolonged high-humidity runs; such conditions are incompatible with anhydride-cure epoxy and moisture-sensitive polyurethane systems. Nitrogen blanketing or sealed tote dosing is required where water content below 0.05 wt% is specified.
Alkaline hard-surface cleaners and water-based degreasers incorporate DOWANOL™ DPM as a coupling solvent between aqueous builders, nonionic surfactants, and hydrophobic fragrance or terpene fractions. Cleaning performance under ASTM D4488 shows measurable soil removal on anionic surfactant systems when the solvent is present at 2–7 wt%; phase stability at 5–40 °C is checked by freeze-thaw cycling rather than extrapolated from Hansen solubility alone. The surface tension of 28.6 dyn/cm at 25 °C supports wetting of oily soils on stainless steel, while the full water miscibility reduces film streaking after rinse. In plant-scale high-pressure spray equipment, the 3.7 cP viscosity at 25 °C has negligible effect on nozzle pressure drop, but the 75 °C flash point requires standard grounding and ventilation controls in heated cleaning baths above 40 °C. The product is listed under EU REACH CAS 34590-94-8 and U.S. TSCA; however, it is not a drop-in replacement for ethylene glycol butyl ether when fast room-temperature evaporation is required because of the 0.02 relative evaporation rate.
When DPM Replaces Butyl Glycol in Aqueous Ink Systems, What Changes in Drying and Odor Profile?
In flexographic and gravure water-based ink concentrates, replacement of ethylene glycol butyl ether with DOWANOL™ DPM alters press-side drying in ways that are measurable by dry-time tests and residual solvent analysis. Because the vapor pressure at 20 °C is 0.4 mm Hg, compared with above 0.8 mm Hg for many butyl glycol formulations, printed film exiting an interstation dryer may retain more solvent at equivalent web speed. Press-ready viscosity is typically maintained at 15–25 s on a Shell or Zahn cup; DOWANOL™ DPM can be added at 1–3 wt% of total formulation to improve resolubility on anilox rolls without increasing ammonia demand. Print gloss and rub resistance under ASTM D5264 require rebalancing of acrylic emulsion coalescence because DPM’s slower release can extend open time but also soften the film if retained above 200 ppm in the final dry ink. Color strength on polyethylene film is evaluated by internal spectrophotometric methods. The odor profile shifts from the sharper ether notes of butyl glycol to a milder sweet ether character, but headspace analysis by GC-MS is required where residual odor in food-contact packaging is a critical control point. Published data for specific ink binders is limited.
In high-speed coil coating of aluminium and steel strip, DOWANOL™ DPM functions as a retarder solvent to prevent solvent popping and vapor entrapment in blocked urethane or polyester-melamine topcoats. Lines running roll-coater application at 150–200 m/min require a boiling range high enough to avoid premature flash in the coater room but volatile enough to leave the film before the final oven zone at 260–280 °C peak metal temperature. DPM at 5–10 wt% of total solvent mass is introduced into letdown batches equipped with variable-speed propellers; the viscosity response is verified with ASTM D4212 dip cups and by cone-and-plate rheology under ASTM D4287. Solvent popping defects on cured panels are assessed by visual inspection under ASTM D714 blister grading. Compared with PM, the slower evaporation of DPM reduces oven entrance viscosity sag, but if line speed drops below 120 m/min, retained solvent can produce pinholes in the final cured film. Published data for high-speed coil coating lines with specific resin systems is limited.
A Three-Solvent Volatility Gradient Distinguishes the Propylene Glycol Methyl Ether Homologs
Selection among the three propylene glycol methyl ether homologs is governed primarily by evaporation-rate and flash-point differences.
| Property | DOWANOL™ PM | DOWANOL™ DPM | DOWANOL™ TPM |
|---|---|---|---|
| CAS Registry Number | 107-98-2 | 34590-94-8 | 25498-49-1 |
| Molecular Weight | 90.1 g/mol | 148.2 g/mol | 206.3 g/mol |
| Boiling Point or Range | 120 °C | 182–192 °C | 242 °C |
| Flash Point, Closed Cup | 31 °C | 75 °C | 121 °C |
| Vapor Pressure at 20 °C | 12.5 mm Hg | 0.4 mm Hg | 0.03 mm Hg |
| Relative Evaporation Rate, nBuAc = 1 | 0.7 | 0.02 | 0.002 |
These comparative values are typical data and not specifications. DOWANOL™ DPM is selected when complete coalescence or tail-solvent retention is required beyond the capability of PM, but where the residual film-softening risk of TPM is considered excessive for fast turnaround packaging lines. The 75 °C closed-cup flash point also permits storage under less stringent flammable-liquid controls than PM, although the flash point is below the 93 °C upper boundary for NFPA 30 Class IIIA combustible liquids. The vapor pressure of 0.4 mm Hg at 20 °C places the product in the low-volatility range for indoor coating operations but does not eliminate the need for local exhaust ventilation in heated flash-off zones.
Prolonged storage in unlined carbon steel at temperatures above 35 °C may increase iron contamination and color drift; stainless steel, aluminium, or lined steel is therefore preferred for bulk storage.